Professional Documents
Culture Documents
Epoxy Phenolic Tank Lining Test Type Cathodic Disbondment Test Method ASTM G42 - "Cathodic Disbondment of Pipeline Coatings Subjected to Elevated Temperature" Specification Details 2 x 100m dft applied directly to Sa2 blasted steel. Typical Results No coating disbondment following 30 days exposure at 60C, 80C and 90C
No blistering, cracking, rusting , adhesion loss and underfilm corrosion following 648 hours exposure to cold wall.
Condensation
Immersion
Immersion
NACE TM-01-74 "Methods for the evaluation of linings for immersion service 90C deionised water"
2 x 100m dft applied directly to Sa2 blasted steel. (stoved & unstoved @ 220C)
Adhesion
ISO 4624 - "Pull-off test for adhesion" using portable adhesion testers
Not less than 10MPa (1450psi) when using a PAT Model GM01 hydraulic adhesion tester on 5mm thick steel.
03 December 2002
Page 1 of 2
All representation and statements concerning the product(s) in this report are accurate to the best of our knowledge. Any statements herein are not intended to be specific recommendations or warranties of any product, combination of products or fitness for purpose
Interline 399
Test Method ASTM D2794 "Resistance to the Effects of Rapid Deformation (Impact)"
03 December 2002
Page 2 of 2
All representation and statements concerning the product(s) in this report are accurate to the best of our knowledge. Any statements herein are not intended to be specific recommendations or warranties of any product, combination of products or fitness for purpose
Interline 399