R.S.T.

Methodology

Material rubbing alcohol . 1 Robinsons Plastic ( 5'' x 5'') . 1 Shopwise Plastic ( 5'' x 5'') . 1 SM Southmall Plastic (5'' x 5'') . Microwavable Plastic ( 3 pcs ) . Procedure 1. Cut the plastic into 5''x 5''. 2. Soak the 3 different biodegradable plastic to 2cm microwavable Plastic. 3. Observe the 3 different biodegradable plastic day by day for two weeks . Hypothesis The reasechers seek to prove the following hypothesis 1. There will be change in its color. 2. Robinsons plastic will degrade faster.