Creep-resistant-steels for high temperature service are those suitable for
applications that require exposures between 345 and 815 0C (650 and 1500
0
F). For each one of the approved materials the usual Code establishes the
allowable design stress at service temperature.
The following Table lists a few Creep-resistant-steels usually considered for
use in the specified temperature ranges.
Table
Creep Resistant Steels
ASME No.

Composition %

Temperature Range

Cr

Mo

SA 204, grade C

--

0.5

430-510

800-950

SA 302, grade B

--

0.5

430-510

800-950

SA 387, grade 12, class 1

1.0

0.5

455-565

850-1050

SA 387, grade 12, class 2

1.0

0.5

345-480

650-900

SA 387, grade 11, class 1

1.25

0.5

455-565

850-1050

SA 387, grade 11, class 2

1.25

0.5

345-480

650-900

SA 387, grade 22, class 1

2.25

1.0

455-595

850-1100

SA 387, grade 22, class 2

2.25

1.0

370-480

700-900

SA 387, grade 5, class 1,


class 2

5.0

0.5

480-620

900-1150

SA 387, grade 9

9.0

1.0

510-595

950-1100

SA 387, grade 91 (1)

9.0

1.0

540-650

1000-1200

SA 240 Austenitic (2)

(2)

(2)

595-815

1100-1500

(1) + Ni, V, Nb, N, Al


(2) - Austenitic Stainless Steels:
Grade 304H 18Cr-8Ni
Grade 316H 16Cr-12Ni-2Mo
Grade 321H 18Cr-10Ni-Ti
Grade 347H 18Cr-10Ni-Nb