You are on page 1of 3

High-arsenic copper concentrates

Posted by John On February 23, 2016 0 Comment

David Duckworth of consulting company Saint Barbara notes that the issue of high-arsenic (high-As) copper
concentrates has been highlighted recently with the start-up of a number of new projects producing this
material.
Copper concentrates can be divided into clean or complex types, he writes in the companys latest
newsletter. The main impurities (deleterious or penalty elements) in complex concentrates are Sb, As, Bi,
Cd, Cl, F, Pb, Hg, U and Zn. Each element has a threshold level above which a smelter will charge a penalty in
addition to treatment/refining charges (TC/RCs). There may also be an upper limit over which the smelter
will reject the concentrate. Penalty charges exist to cover the extra costs incurred by the smelter in
processing and safely storing contaminated (deleterious) materials.
In 2014/15, production of complex concentrate increased significantly and the volume of complex
concentrates available on the market is expected to rise by 700% between 2013 and 2016. New mines, such
as Toromocho in Peru (1% As) and Ministro Hales in Chile (4% As), are producing complex concentrates,
while As content in concentrates produced at existing mines, including Marcapunta in Peru (8% As),
Chelopech in Bulgaria (6% As) and Chuquicamata in Chile (1.2% As), has risen.
Around 30% of world copper concentrates output contains more than 0.1% or 1,000 ppm As. complex
copper concentrates have an As content greater than 0.2% (2,000 ppm) with no upper limit, although China
imposes a limit of 0.5% As (5,000 ppm) on imported base metal concentrates.
Many copper smelters able to process dirty or complex concentrates prior to the 1990s, have either
stopped this practice or closed for environmental reasons. These smelters include La Oroya in Peru, San Luis
de Potosi in Mexico, Tacoma in the USA, Rnnskr in Sweden, PASAR in the Philippines and Kosaka in Japan.
Currently only a few copper smelters Tsumeb in Namibia (see map), Altonorte in Chile, Guixi in China and
Horne in Canada can process complex concentrates and Tsumeb is the only option for large volumes of
very high-As concentrates, with >1% As. These smelters will charge a penalty to treat high-As concentrate,
while Tsumeb charges higher TCs to treat complex concentrates.
In the past, Godfrey and Nicholas-Herreschoff roasters were often used to fume off the As in very high-
grade com-plex concentrates to produce arsenic trioxide (As2O3) and calcined copper concentrate with a
much reduced As content. Roasters were either located at the mine site or adjacent to a smelter. The only
such roasters in operation to-day are those at Tsumeb.
Codelco has installed an Outotec Partial Roaster at its Ministro Hales mine to reduce the As content of the
copper concentrates. The fluid bed partial roaster processes high-As copper concentrate to produce a
calcine with a low As content and high-copper concentrate. The roaster complex has an integrated effluent
plant which removes the As content from the process water. Effluent is treated using calcium arsenite
precipitation.
Blending is the most common solution to the problem of treating high-As content in copper concentrates,
where high-As concentrate is mixed with clean copper concentrate to dilute the As content to acceptable
levels for smelters. As there are only four smelters worldwide which can treat high-As material, capacity is
limited. Since 2014, the volume of high-As concentrate has exceeded treatment capacity in smelters.
During 2014, Codelco set up a strategic alliance with Ocean Partners to blend high-As copper concentrate
from its Ministro Hales mine with clean third-party concentrate(s) bought in by both companies, at Ocean
Partners concentrate blending facility in Taiwan. As the blended concentrate grades less than the Chinese
custom cap of 0.5% As, it can be sold to Chinese smelters.
EcoMetales Copper Flue Dust Treatment Plant (PTPA for its acronym in Spanish) and Arsenic and Antimony
Abatement Process (PAAA for its acronym in Spanish), located near Calama in Chile, treat smelter flue dust,
refinery effluent and other solid hazardous wastes from Codelcos Chuquicamata, Potrerillos (Salvador) and
Ventanas smelter and refinery complexes. These products may contain up to 30% Cu and deleterious levels
of As (5-17%), bismuth and antimony. In the PTPA plant, dust is acid leached to produce copper pregnant
leach solution which is pumped 7km to Codelcos Chuquicamata mine, where it is used to produce copper
cathodes. The leaching waste (with 7% Cu) is dried and conditioned before being sent to the Chuquicamata
smelter for processing.
The PAAA plant treats copper-rich solution produced by the PTPA and leached waste from the PTPA, to
recover copper, together with scorodite (FeAsO42H2O), the environmentally stable form of As. The
scorodite is disposed of at a site 1km from the plant, which meets all environmental standards.
Several hydrometallurgical technologies atmospheric leaching, bio-oxidation and pressure leaching
are available for processing high-As concentrates. Few have achieved commercial application.
One example is CESL high pressure oxidation technology, promoted by Teck Aurubis. A small industrial scale
plant operated successfully from 2008 to 2010 for Vale in the Carajs region of Brazil. It is claimed that more
than 99% of the As remains undissolved in the leach residue. The copper is dissolved and follows a
conventional SX/EW route to cathode. Gold in the concentrate reports to the leach residue from which it
can be extracted by cyanidation with little or no dissolution of As. Silver could be treated similarly,
although the quantity reporting to the leach residue is not determined.
In the short and medium term, the problem of high-As copper concentrates will be alleviated somewhat by
Codelcos roaster reaching full capacity, the decline in the As level in the Toromocho concentrate, new mine
capacity coming on-stream producing clean concentrates and a possible expansion at Tsumeb.
In the long term, however, the trend towards the exploration of more difficult deposits will continue.
Although these new projects will be delayed due to copper price decline, many of them will produce
concentrates with elevated levels of As.
The problem of treating high-As concentrate is not going to go away and will be overcome by continued
blending, use of existing technology and the development of new technology.

http://im-mining.com/2016/02/23/high-arsenic-copper-concentrates/