You are on page 1of 2

12/1/2018 Elcometer launch an equivalent tape for ASTM D3359 Cross Cut Adhesion Test Press Release July

Test Press Release July 2010

EN Search...

Blast Equipment Inspection Equipment Laboratory & Physical Test Equipment About

Home
Elcometer launch an equivalent tape for ASTM D3359 Cross Cut Adhesion Test Press Release July 2010

Elcometer launch an equivalent tape for ASTM D3359 Cross Cut


Adhesion Test Press Release July 2010

Manchester, UK July 2010 – Elcometer is pleased to announce the launch of


its Elcometer 99 tape as a replacement for the Permacel P99 tape which is
used in accordance with ASTM D3359 – the cross cut adhesion test method
for measuring adhesion using the tape test.

Following independent testing of the Elcometer 99 tape versus rolls of


Permacel P99 tape (both within and outside of the tape’s expiry date) and
another two possible alternate tapes proposed by the ASTM D01.23 Sub-Committee responsible for the
D3359 Standard test method, the Elcometer 99 Tape, unlike the others tested, has been proven to be a very
close equivalent to the Permacel P99 tape which was withdrawn from production by the manufacturer in mid
2009.

The independent testing also identified how the Permacel P99 tape’s adhesive properties changes when used
outside its expiry date. It is clear that as Permacel P99 adhesive tape has a 12-month shelf life – making
any remaining tape valid until July 2010 – finding a replacement tape was urgently required in order to
maintain this important adhesion test.

Elcometer commissioned a tape manufacturer to make a close equivalent to the Permacel P99 tape and the
Elcometer 99 tape was produced.

The testing was carried out using samples of Permacel P99 tape taken from a roll of tape that has a shelf life
that expires in July 2010 and a roll of tape that had already expired. The two other tapes in the trial had
been proposed as alternatives to the Permacel P99 tape and were the Scapa 8010-B tape and the Intertape
LA-26 tape. The samples of these tapes were taken from rolls that were within their shelf life. Both of these
tapes are established products for uses other than adhesion testing but were said by the suppliers to be
near equivalents to the Permacel P99 tape.

The independent test results in Table 1 clearly show that on average the Elcometer 99 tape has a peel
adhesion strength that is within 4% of the average peel strength of the Permacel P99 tape. The alternative
tapes are 67.8% higher and 21.4% lower than the average for the Permacel P99 tape making the Elcometer
99 tape the closest match for the tapes that were tested.

https://www.elcometer.com/en/elcometer-launch-an-equivalent-tape-for-astm-d3359-cross-cut-adhesion-test-press-release-july-2010.html 1/2
12/1/2018 Elcometer launch an equivalent tape for ASTM D3359 Cross Cut Adhesion Test Press Release July 2010

WHAT'S NEW SERVICE & SUPPORT

Request a Catalogue

Videos

Service & Technical Support

Extend Your Warranty

Software Downloads

International Standards

Product List

COMPANY CONTACT

About Elcometer

Company Policies

Terms & Conditions

Quality & ISO Certification

Careers

Exhibition Calendar

Blast Equipment Inspection Equipment Laboratory & Physical Test Equipment About

Login Press Sitemap Privacy Policy Copyright © Elcometer Limited 2018

https://www.elcometer.com/en/elcometer-launch-an-equivalent-tape-for-astm-d3359-cross-cut-adhesion-test-press-release-july-2010.html 2/2

You might also like