Hubungan Porositas dan Kandungan Clay terhadap Kecepatan Gelombang

Pada Tekanan 20 MPa

Vp= 5,49 - 6,94Ø - 2,17C


Vs= 3,39 - 4,73Ø - 1,81C

No Porositas (%) Kandungan Clay (%) Kecepatan Primer (km/s) Kecepatan Sekunder (km/s)
1 5% 0% 5.143 3.154
2 5% 10% 5.132 3.144
3 5% 20% 5.121 3.135
4 5% 30% 5.110 3.126
5 5% 40% 5.100 3.117
6 5% 50% 5.089 3.108
7 10% 0% 4.796 2.917
8 10% 10% 4.774 2.899
9 10% 20% 4.753 2.881
10 10% 30% 4.731 2.863
11 10% 40% 4.709 2.845
12 10% 50% 4.688 2.827
13 15% 0% 4.449 2.681
14 15% 10% 4.416 2.653
15 15% 20% 4.384 2.626
16 15% 30% 4.351 2.599
17 15% 40% 4.319 2.572
18 15% 50% 4.286 2.545
19 20% 0% 4.102 2.444
20 20% 10% 4.059 2.408
21 20% 20% 4.015 2.372
22 20% 30% 3.972 2.335
23 20% 40% 3.928 2.299
24 20% 50% 3.885 2.263
25 25% 0% 3.755 2.208
26 25% 10% 3.701 2.162
27 25% 20% 3.647 2.117
28 25% 30% 3.592 2.072
29 25% 40% 3.538 2.027
30 25% 50% 3.484 1.981
31 30% 0% 3.408 1.971
32 30% 10% 3.343 1.917
33 30% 20% 3.278 1.862
34 30% 30% 3.213 1.808
35 30% 40% 3.148 1.754
36 30% 50% 3.083 1.700